Precise and Reliable DSC Results for Pharmaceuticals, Foods and Cosmetics

The instrument serves for the investigation of:

  • Melting temperatures and enthalpies of fusion
  • Polymorphism (ability of a solid substance to exist in multiple forms or crystal structures)
  • Crystallization temperatures and enthalpies
  • Glass transitions (characteristic for amorphous areas or amorphous substances)
  • Solid-solid interactions (e.g., between ingredients in a physical mixture)
  • Phase diagrams
  • Eutectic purity
  • Solid-fat content (SFC)
  • Reaction temperatures and enthalpies
  • Specific heat capacity (cp)
  • Cross-linking reactions (curing)
  • Oxidation-induction time and temperature  (OIT (isothermal), OIT (dynamic), OOT)

Key Features:

  • Software which actively supports you – AutoEvaluation and Identify
  • Various sensor types to adapt instrument to different application needs
  • Excellent sensitivity and high resolution
  • Automatic sample tray identification
  • Measuring methods independent of instrument
  • Efficient and cost-effective cooling – In pharmacy, cosmetics and food, most DSC instruments are equipped with a mechanical cooling system (intracooler). However, if very low start temperatures are required, a liquid nitrogen cooling device can be simultaneously connected to the DSC 204 F1 Nevio. In this case, the LN2 cooling will only be activated at temperatures below -85°C, which reduces the liquid nitrogen consumption considerably.